i didn't research the krylon triple thick glaze product thoroughly enough before using it and i had all of the negative experiences listed on here except the blistering in the sun. the first coat did go on cloudy. i was excited when it dried (or so i thought it dried) to an excellent deep, rich clear coat. my biggest issue is that the stuff just doesn't seem to dry. even after two days hanging in a 70 degree room with low humidity (close to ideal drying conditions i would think) the terrycloth pattern of the towel i laid it on to polish it was imprinted on the back of the guitar. i cleaned it up and re-sprayed it and the full dry time is yet to be seen. will repost with results after i give it a week or so to cure and let everyone know how i made out.